I opened a new package of Hatchbox white PLA and put it in my dryer for 2 hours. The first print was covered in pock marks. Thinking it might still be wet I did 2 cycles of 6 hour drying and printed again. The pock marks were more widespread but the result is still an unusable print. Subsequent prints using other PLA were fine. I ordered it >30 days ago and I wonder if they’ll stand behind the product. If not, bye bye HB.